In order to avoid stress corrosion cracking of forged flanges, the following measures can be taken: Choose the right material: Choosing a material with good resistance to stress corrosion cracking is the first step in prevention. Materials with high corrosion resistance, such as stainless steel and acid-resistant alloys, should be selected according to the characteristics of the working environment and the medium. Control the stress state: Reasonable material design and manufacturing process can reduce or eliminate the internal stress in the forged flange. In the forging process, attention should be paid to controlling the cooling rate and temperature gradient to avoid stress concentration caused by rapid cooling of forged parts. Reduce stress: Through heat treatment and other ways, the forged flange is annealed or tempered to eliminate or reduce the internal stress, so as to improve its resistance to stress corrosion cracking. Control environment: For the presence of high corrosive media or atmosphere in the working environment, appropriate protective measures should be taken, such as using anti-corrosion coating, keeping the environment dry, avoiding strong acids and alkalis. Regular inspection and maintenance: regular inspection of forged flanges, especially the parts exposed to corrosive media, focus on observation, timely detection of possible signs of corrosion, and take necessary maintenance measures. It should be noted that the above measures are only general recommendations, and specific prevention and control measures should be formulated according to the actual working environment, media and material characteristics of the flange. In specific projects, it is recommended to consult a professional engineer or an expert in the relevant field for more detailed and targeted advice.